Electronic Components Datasheet Search
  English  ▼

X  

HS1 Datasheet(PDF) 39 Page - Clarke International

Part # HS1
Description  MIG/MMA/TIG INVERTER WELDER
PDF  48 Pages
Scroll/Zoom Zoom In 100%  Zoom Out
Manufacturer  CLARKE [Clarke International]
Direct Link  https://www.clarkeinternational.com/
Logo CLARKE - Clarke International

HS1 Datasheet(HTML) 39 Page - Clarke International

Back Button HS1 Datasheet HTML 35Page - Clarke International HS1 Datasheet HTML 36Page - Clarke International HS1 Datasheet HTML 37Page - Clarke International HS1 Datasheet HTML 38Page - Clarke International HS1 Datasheet HTML 39Page - Clarke International HS1 Datasheet HTML 40Page - Clarke International HS1 Datasheet HTML 41Page - Clarke International HS1 Datasheet HTML 42Page - Clarke International HS1 Datasheet HTML 43Page - Clarke International Next Button
Zoom Inzoom in Zoom Outzoom out
 39 / 48 page
background image
39
Parts & Service: 020 8988 7400 / E-mail: Parts@clarkeinternational.com or Service@clarkeinternational.com
TROUBLESHOOTING
Your welder has been designed to give long and trouble free service. If however,
having followed the instructions in this booklet carefully you still encounter problems,
the following points should help identify and resolve them.
DEFECT
CAUSES
SUGGESTIONS
Spark will not start
Bad clamp connection.
Inverter PCB defective.
Check clamp connection.
Contact your nearest CLARKE
dealer.
No output voltage
Overheated machine
Wait for thermal cutout to be
reset.
Internal relay has failed.
Contact your nearest CLARKE
dealer.
Inverter PCB defective.
Contact your nearest CLARKE
dealer.
Wrong output
current
Current selector control is
defective.
Contact your nearest CLARKE
dealer.
Low power supply voltage.
Have electrician check the
mains supply.
Porosity of welds
Acid electrode on steel with
high sulphur content.
Electrode oscillates too much.
Workpieces are too far apart.
Workpiece being welded is
cold.
Use basic electrode.
Move edges to be welded
closer together. Move slowly at
the beginning.
Cracks in weld
Material being welded is dirty
(e.g.oil, paint, rust, oxides,
moisture).
Incorrect current/voltage.
Clean workpiece before
welding is an essential method
of achieving neat weld beads.
Also increase current output.
Poor penetration
Low welding current, high
welding rate,
Poor electrode inclination angle
or too far from workpiece.
Ensure operating parameters
are regulated and improve
preparation of work pieces.
Profile defects
Welding parameters are
incorrect.
Pass rate is not related to
operating parameter
requirements.
Electrode not inclined
constantly while welding.
Follow basic and general
welding principles.



Html Pages

1 2 3 4 5 6 7 8 9 10 11 12 13 14 15 16 17 18 19 20 21 22 23 24 25 26 27 28 29 30 31 32 33 34 35 36 37 38 39 40 41 42 43 44 45 46 47 48


Datasheet Download

Go To PDF Page


Link URL



Does ALLDATASHEET help your business so far?  [ DONATE ] 

About Alldatasheet   |   Advertisement   |   Contact us   |   Privacy Policy   |   Link to Datasheet    |   Link Exchange   |   Manufacturer List
All Rights Reserved©Alldatasheet.com


Mirror Sites
English : Alldatasheet.com  |   English : Alldatasheet.net  |   Chinese : Alldatasheetcn.com  |   German : Alldatasheetde.com  |   Japanese : Alldatasheet.jp
Russian : Alldatasheetru.com  |   Korean : Alldatasheet.co.kr  |   Spanish : Alldatasheet.es  |   French : Alldatasheet.fr  |   Italian : Alldatasheetit.com
Portuguese : Alldatasheetpt.com  |   Polish : Alldatasheet.pl  |   Vietnamese : Alldatasheet.vn
Indian : Alldatasheet.in  |   Mexican : Alldatasheet.com.mx  |   British : Alldatasheet.co.uk  |   New Zealand : Alldatasheet.co.nz
Family Site : ic2ic.com  |   icmetro.com