Electronic Components Datasheet Search
  English  ▼

X  

AN2639 Datasheet(PDF) 11 Page - STMicroelectronics

Part # AN2639
Description  Soldering recommendations and package information for Lead-free ECOPACK microcontrollers
PDF  15 Pages
Scroll/Zoom Zoom In 100%  Zoom Out
Manufacturer  STMICROELECTRONICS [STMicroelectronics]
Direct Link  http://www.st.com
Logo STMICROELECTRONICS - STMicroelectronics

AN2639 Datasheet(HTML) 11 Page - STMicroelectronics

Back Button AN2639 Datasheet HTML 7Page - STMicroelectronics AN2639 Datasheet HTML 8Page - STMicroelectronics AN2639 Datasheet HTML 9Page - STMicroelectronics AN2639 Datasheet HTML 10Page - STMicroelectronics AN2639 Datasheet HTML 11Page - STMicroelectronics AN2639 Datasheet HTML 12Page - STMicroelectronics AN2639 Datasheet HTML 13Page - STMicroelectronics AN2639 Datasheet HTML 14Page - STMicroelectronics AN2639 Datasheet HTML 15Page - STMicroelectronics  
Zoom Inzoom in Zoom Outzoom out
 11 / 15 page
background image
DocID14016 Rev 4
11/15
AN2639
Dry packing
6
Dry packing
Quality and reliability of SMDs after soldering depends heavily on moisture absorption
during storage. A specific packing, called dry pack, was implemented for defined conditions
at the delivery. Time and environment will modify the amount of absorbed humidity. Moisture
sensitive SMDs (SOP, PLCC, PQFP, BGA, VFQFPN, UFQFPN, and WLCSP) are dry
packed to protect them from moisture absorption during shipment / storage and then to
reduce failure risks mainly due to popcorn effect.
6.1
Pop-corn effect
Pop-corn effect is the cracking of the package during the soldering cycle. It has got a
growing importance due to the trends towards larger die size in integrated circuits. This
phenomenon is mainly caused by the moisture absorbed by the epoxy molding. When the
package is exposed to high temperatures, as in most SMT soldering processes, the water at
the interface between plastic and die pad vaporizes suddenly, generating high internal
pressure. Cracks may occur in the molding compound depending on the absorbed moisture
level, soldering temperature and time, die size, package structure and molding compound
characteristics.
SMD products are contained in tubes, on trays or on tape, and are then vacuum sealed in
an hermetic bag.
Opening the package will stop the ideal conditions and start the influence of the normal
environment. Figure 6 shows the recommended handling flow.



Html Pages

1 2 3 4 5 6 7 8 9 10 11 12 13 14 15


Datasheet Download

Go To PDF Page


Link URL



Does ALLDATASHEET help your business so far?  [ DONATE ] 

About Alldatasheet   |   Advertisement   |   Contact us   |   Privacy Policy   |   Link to Datasheet    |   Link Exchange   |   Manufacturer List
All Rights Reserved©Alldatasheet.com


Mirror Sites
English : Alldatasheet.com  |   English : Alldatasheet.net  |   Chinese : Alldatasheetcn.com  |   German : Alldatasheetde.com  |   Japanese : Alldatasheet.jp
Russian : Alldatasheetru.com  |   Korean : Alldatasheet.co.kr  |   Spanish : Alldatasheet.es  |   French : Alldatasheet.fr  |   Italian : Alldatasheetit.com
Portuguese : Alldatasheetpt.com  |   Polish : Alldatasheet.pl  |   Vietnamese : Alldatasheet.vn
Indian : Alldatasheet.in  |   Mexican : Alldatasheet.com.mx  |   British : Alldatasheet.co.uk  |   New Zealand : Alldatasheet.co.nz
Family Site : ic2ic.com  |   icmetro.com