GWH3 Datasheet(PDF) 32 Page - Clarke International

Part # GWH3
Description  MIG/MMA/TIG INVERTER WELDER
PDF  40 Pages
Scroll/Zoom Zoom In 100%  Zoom Out
Manufacturer  CLARKE [Clarke International]
Direct Link  https://www.clarkeinternational.com/
Logo CLARKE - Clarke International

GWH3 Datasheet(HTML) 32 Page - Clarke International

Back Button GWH3 Datasheet HTML 28Page - Clarke International GWH3 Datasheet HTML 29Page - Clarke International GWH3 Datasheet HTML 30Page - Clarke International GWH3 Datasheet HTML 31Page - Clarke International GWH3 Datasheet HTML 32Page - Clarke International GWH3 Datasheet HTML 33Page - Clarke International GWH3 Datasheet HTML 34Page - Clarke International GWH3 Datasheet HTML 35Page - Clarke International GWH3 Datasheet HTML 36Page - Clarke International Next Button
Zoom Inzoom in Zoom Outzoom out
 32 / 40 page
background image
32
Parts & Service: 020 8988 7400 / E-mail: Parts@clarkeinternational.com or Service@clarkeinternational.com
Loose coils of wire
tangle around wire
drum inside
machine.
Locking knob too slack.
Tighten Locking Knob slightly.
Do not over-tighten.
Erratic wire feed.
Tensioning Knob too tight.
Loosen Tensioning Knob
slightly.
Tension roller worn.
Check and replace if necessary.
Insufficient pressure on
tension roller.
Increase pressure on tension
roller
Caution: DO NOT over-tighten.
Wire dirty, rusty, damp or bent. Re-cut wire and ensure it is
clean.
Liner partially blocked.
Clean with compressed air.
Poor quality welds.
Insufficient gas at weld area.
Check that gas is not being
blown away by draughts and if
so move to a more sheltered
work area. If not, increase gas
supply.
Rusty, painted, damp, oil or
greasy workpiece.
Ensure workpiece is clean and
dry.
Rusty/dirty wire.
Ensure wire is clean and dry.
Poor earth contact.
Check earth clamp/workpiece
connection.
Welder cuts out
whilst in use.
Duty cycle exceeded (auto cut-
out operates).
Allow welder to cool 15-30
mins before continuing.
Note: If duty cycle is
continually exceeded, damage
to the welder may result and
welder output is probably too
small for application.
DEFECT
CAUSES
SUGGESTIONS



Html Pages

1 2 3 4 5 6 7 8 9 10 11 12 13 14 15 16 17 18 19 20 21 22 23 24 25 26 27 28 29 30 31 32 33 34 35 36 37 38 39 40


Datasheet Download

Go To PDF Page


Link URL



Does ALLDATASHEET help your business so far?  [ DONATE ] 

About Alldatasheet   |   Advertisement   |   Contact us   |   Privacy Policy   |   Link to Datasheet    |   Link Exchange   |   Manufacturer List
All Rights Reserved©Alldatasheet.com


Mirror Sites
English : Alldatasheet.com  |   English : Alldatasheet.net  |   Chinese : Alldatasheetcn.com  |   German : Alldatasheetde.com  |   Japanese : Alldatasheet.jp
Russian : Alldatasheetru.com  |   Korean : Alldatasheet.co.kr  |   Spanish : Alldatasheet.es  |   French : Alldatasheet.fr  |   Italian : Alldatasheetit.com
Portuguese : Alldatasheetpt.com  |   Polish : Alldatasheet.pl  |   Vietnamese : Alldatasheet.vn
Indian : Alldatasheet.in  |   Mexican : Alldatasheet.com.mx  |   British : Alldatasheet.co.uk  |   New Zealand : Alldatasheet.co.nz
Family Site : ic2ic.com  |   icmetro.com